Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.348 GPa | 340.6 ksi | ASTM D638 |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |