Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.79 MPa | 839 psi | |
Momentive Performance Materials RTV88 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Tensile Strength, Ultimate | 5.78 MPa | 839 psi | ASTM D638 |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |