EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 40% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by the following key-properties: high stiffness and strength even after conditioning and over a wide temperature rangeexcellent notched impact resistance also at low temperatureslow creephigh heat distortion temperaturesgood dimensional stability and little warpagegood surface appearance and ease of processing The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement. Grilon TSGL-40/4 FA black 9840 is used in the following market segments: mechanical engineeringhousehold and appliances The glass-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm). Grilon TSGL-40/4 FA black 9840 is according to NSF- 61 standard suitable for all engineering thermoplastic applications with the requirements of approvals in contact with foodstuff or/and in contact with drinking water. Certified for a maximum surface area to volume ratio of 250 sq.in./LInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 1.80 %
1.80 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 185 MPa
26800 psi
conditioned; ISO 2039-1
280 MPa
40600 psi
dry; ISO 2039-1
Tensile Strength at Break 160 MPa
23200 psi
conditioned; ISO 527-1/-2
220 MPa
31900 psi
dry; ISO 527-1/-2
Elongation at Break 2.1 %
2.1 %
dry; ISO 527-1/-2
2.5 %
2.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 10.0 GPa
1450 ksi
conditioned; ISO 527-1/-2
13.5 GPa
1960 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
5.50 J/cm²

@Temperature 30.0 °C
26.2 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
dry; ISO 179/1eA
3.00 J/cm²
14.3 ft-lb/in²
conditioned; ISO 179/1eA
2.50 J/cm²

@Temperature 30.0 °C
11.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 120 °C
230 - 248 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 225 °C
437 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 22.0 kV/mm
559 kV/in
conditioned; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Exterior
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Long Fiber Reinforced
Special Characteristics Improved heat resistance
Water Contact NSF 61