Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® 940 NC010 PET  (Unverified Data**)
Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXR123R PC (Europe-Africa-Middle East)
Lexan FXR123R Resin
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 3400F Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs ..
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ N1000A-M41 Nylon
Standard unreinforced injection grade. Main features:Low water absorptionChemical ResistanceExamples of application are:Friction and wear applicationGear and Wheel
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East)
NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 23.0 - 150 °C
33.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP
LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66
LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
dry; ISO 11359-1/-2
DSM Akulon® S223-PG8 PA66-GF40
40% Glass Reinforced, Impact Modified
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
DSM Arnite® TV4 461 (PBT+PET)-GF30
30% Glass Reinforced
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
DSM Arnite® TV4 461 KL (PBT+PET)-GF30
30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GTR 45 PA6I/6T
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides..
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40
Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance..
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR XE 4139 black 9231 PA*
Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a..
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry)
Information provided by BASF
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin
GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..