Material Notes:
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: outstanding impact resistance even at low temperaturesvery high flexural fatigue strengthgood chemical- and stress-crack resistancehigh UV resistancecan be colored in transparent as well as opaque colors Grilamid TR 90 NZ shows reversible thermotropic transparency. The transparency continuously decreases during heating from room temperature to about 70°C. At 80°C the material is opaque. Grilamid TR 90 NZ is suitable for production of optical and technical demanding parts in the application fields of: OpticsElectroElectronicsAutomotiveMechanical engineeringDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 3.0 %
3.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
conditioned; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
conditioned; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
120 °C
248 °F
short term; EMS
Transformation Temperature, Tg 155 °C
311 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Automotive Compressed air systems
Exterior
Fuel systems
Interior
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Optics Spectacle frames
Processing Injection Molding
Other Extrusion
Product Attributes Co Polyamide
Hydrolysis resistant
Transparent Polyamide
Special Characteristics High impact or impact modified
Improved UV resistance (outdoor use)
Transparent