Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.30 GPa | 189 ksi | |
Radici Radilon® A HS (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East) LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BF330MO Polypropylene Copolymer BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis BJ380MO Polypropylene Copolymer BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 1mm/min; ISO 527-2 |
Borealis HB205TF Polypropylene HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 572-2 |
Total Lumicene® MR30MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding Lumicene® MR30MX0 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection and injection stretch blow molding. Lumicene® MR30MX0 differs from the other random copolyme.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ASTM D638 |
Total PPR 6523WZ Polypropylene, Nucleated Random Copolymer for Injection Molding Impact - 6523WZ produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat - 6523WZ contains an antistat to help protect molded parts from dust acc.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | |
Covestro Baydur® GS PUR Polyurethane Polyurethane casting system for the production of solid components. Pressureless casting into open or closed molds, fast demold times, good rot resistance. Combines easily with other materials.Infor.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 HWV0CP Nylon 6, Flame Protection, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | Foaming Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following .. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture) Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Tensile Modulus | 1.30 GPa | 189 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |