Parker Chomerics T-Wing™ Heat Spreader

Category Other Engineering Material
Manufacturer Parker Chomerics
Trade Name T-Wing™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics T-Wing™ Heat Spreader.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of flexible copper foil sandwiched between electrically insulating filmsInformation provided by Chomerics
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Insulator Thickness
50.8 microns
2.00 mil
PSA Thickness
178 microns
7.00 mil
Thermal Conductor Thickness
330 microns
13.0 mil
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 12.11 kV/mm
307.7 kV/in
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Binder Black
Insulator Polyester
Pressure-sensitive adhesive system Polyester film (glossy black)
Thermal Conductor Copper
Weight (oz/in^2) 0.039