Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® 723-1, Extrusion Grade
(discontinued **) Extrusion grade for refrigerator inliner.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® QE 1030, Extrusion Grade
(discontinued **) Extrusion grade for food contact applications, improved tear propagation resistance.Applications: Lids for margarine tubs.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005... |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® QE 1120, Extrusion Grade
(discontinued **) General purpose extrusion grade.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL B733/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,095-04-35-15 Very high impact resistant grade for sheet extrusion with good processability and high thermal sta.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL PD H330/S ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 Injection moulding grade with high flow and gloss, specially developed to meet the requirements of.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PE 5902 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM HO TL2 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® ABS CR X BK Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceUses: Electrical PartsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F126-C Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K222-D (Dry) Low Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 H FR PA12 FR Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS Developmental productGrade with improved low-temperature impact strength and petrol resistance for automotive partsin version BBS904 suitable for extrusion/extrusion blow molding and electroplating .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® QE 1122, Injection Grade
(discontinued **) Injection molding grade, very high impact combined with high modulus, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEO.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K225-KS Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |