Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 243-1 |
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0 Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | K20/P50; IEC 60243-1 |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | VDE 0303/4 |
Polyram RamSter PF300G6 PBT, 30% Glass Fiber 30% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
DuPont Performance Polymers Hytrel® 40CB Polyester Elastomer TPC-ET
(Unverified Data**) Black Polyester Elastomer Concentrate Developed for Protection Against Light DegradationInformation provided by DuPont Performance Polymers |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |