Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 50% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined with high toughnessHigh elongationVery low water absorptionHydrolysis and chemical resistanceEasy processing, particularly suitable for very thin- or very thick-walled moldings The special composition of Grilamid LBV-50H FWA black 9225 makes it suitable for the direct contact with drinking water up to 85°C as well as foodstuff. Application examples: Grilamid LBV-50H FWA black 9225 is designed for applications predominantly in the following application fields: Robust valves and fittings for water and gas supply.Taps, fittings, meters, pumps in sanitary equipmentDomestic appliances and household goodsComponents in the food processing industryInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Water Absorption 0.80 %
0.80 %
ISO 62
Moisture Absorption 0.400 %
0.400 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
conditioned, 15s; ISO 868
Ball Indentation Hardness 190 MPa
27600 psi
conditioned; ISO 2039-1
Tensile Strength at Break 160 MPa
23200 psi
conditioned; ISO 527-1/-2
170 MPa
24700 psi
dry; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.5 GPa
1810 ksi
conditioned; ISO 527-1/-2
13.5 GPa
1960 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
9.50 J/cm²
45.2 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
9.50 J/cm²

@Temperature 30.0 °C
45.2 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
dry; ISO 179/1eA
1.80 J/cm²
8.57 ft-lb/in²
conditioned; ISO 179/1eA
1.40 J/cm²

@Temperature 30.0 °C
6.66 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.40 J/cm²

@Temperature 30.0 °C
6.66 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 40.0 kV/mm
1020 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Heating systems
Sanitary, water and gas supply
Processing Injection Molding
Product Attributes Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Water Contact ACS
DVGW W270
KTW
NSF 61
WRAS
Users viewing this material also viewed the following: