Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 S20 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
Radici Radilon® SERV3808 K (dry) Nylon 6 Heat stabilized glass-fiber reinforced with high impact strengthInformation provided by Radici group. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B1S25 G50 50% Glass Fiber Reinforced Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ASTM D256 |
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking .. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 30.0 °C |
8.57 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 3959 nat PA610 Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | DIN 53 453 |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Conditioned) Description: Ultramid A3W2G6 BK20560 is a developmental 30% glass fiber reinforced, pigmented black, injection molding PA66/6 with high heat aging resistance.Applications: Automotive power train app.. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin 15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |