Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 TF-GV 1530 Nylon 6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 141 PC (Europe-Africa-Middle East) LEXAN 141 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 163R PC (Europe-Africa-Middle East) LEXAN 163R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 163R is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 261R PC (Europe-Africa-Middle East) LEXAN 261R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV300 990 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East) LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.55 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Thickness 3.00 - 3.00 mm |
6.66 - 7.61 ft-lb/in² @Thickness 0.118 - 0.118 in |
Average value: 1.44 J/cm² Grade Count:16 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179 |
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Borealis Bormod™ BE961MO Polypropylene for Injection Molding Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast .. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 30.0 °C |
6.66 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN 54G35EF BKB336 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced laser markable PPA High Performance Polyamide Developed for Electrical and Electronics Applications. Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabiliz.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | |
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 953A PC (Europe-Africa-Middle East) LEXAN 953A is a high viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |