Material Notes:
Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good transparencyLow melting point (130°C) Grilon CF 6 S is suitable for the manufacture of both flat and blown coextruded films with temperature sensitive polymers such as PVDC and EVOH. Typical applications are cook in bag for meat, cheese, deep-draw consumer and medical packaging and asymmetric barrier film structures.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 120 cc/m²/day
7.73 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
200 cc/m²/day
12.9 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 400 cc-mm/m²-24hr-atm
1020 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
800 cc-mm/m²-24hr-atm
2030 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 180 g/10 min
180 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPa
4060 psi
ISO 527-3
Film Elongation at Break, MD 800 %
800 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 15 %
15 %
ISO 527-3
Film Elongation at Yield, TD 8.0 %
8.0 %
ISO 527-3
Tensile Modulus 0.400 GPa
58.0 ksi
conditioned; ISO 527-1/-2
Tear Strength 65.0 kN/m
371 pli
Trouser Tear resistance MD; ISO 6383-1
65.0 kN/m
371 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 8160 g
8160 g
ISO 6383-2
Elmendorf Tear Strength TD 8160 g
8160 g
ISO 6383-2
Film Tensile Strength at Break, MD 85.0 MPa
12300 psi
ISO 527-3
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 130 %
130 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Gelboflextest [holes/m²], EMS 100
Packaging Oriented film
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
Flexible
High viscosity
Special Characteristics Transparent