Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 28.0 MPa | 4060 psi | ISO 1184 |
SIDPEC EGYPTENE® HD 4602 FA HDPE Film Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official dis.. |
|||
Film Tensile Strength at Yield, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra.. |
|||
Film Tensile Strength at Yield, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Film Tensile Strength at Yield, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Film Tensile Strength at Yield, TD | 28.0 MPa | 4060 psi | ISO 527-3 |
EMS-Grivory Grivory® BM 20 SBG PA* Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther.. |