Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.400 GPa | 58.0 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nima™ HL 18400 HDPE High Density Polyethylene - Halogenated FR compound with good impact resistance. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepa.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 442 Black V PA6, Conditioned Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Tensile Modulus | 0.400 - 0.600 GPa | 58.0 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding Bormed LE6609-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.Bormed LE6609-PH can be used in "blow-fi.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | MD/TD; ISO 527-3 |
Borealis Bormed™ RB801CF Polypropylene Random Copolymer Bormed™ RB801CF is a random copolymer. Applications: Bormed™ RB801CF is intended for packaging for medical devices, pouches, and packaging for pharmaceutical products. Additives: Bormed™ RB801C.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPure™ RD226CF Polypropylene Random Copolymer BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me.. |
|||
Tensile Modulus | 0.400 GPa @Temperature 100 °C |
58.0 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | MD/TD; ISO 527-3 |
Borealis Bormed™ RD808CF Polypropylene Random Copolymer Bormed™ RD808CF is a random copolymer. Applications: Bormed™ RD808CF is intended for packaging for medical devices, thin pouches, and packaging for pharmaceutical products. Additives: Bormed™ R.. |
|||
Tensile Modulus | 0.400 - 0.500 GPa | 58.0 - 72.5 ksi | MD/TD; ISO 527-3 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Tensile Modulus | 0.400 GPa @Temperature 80.0 °C |
58.0 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | ISO 527-2 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Tensile Modulus | 0.400 - 0.600 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
58.0 - 87.0 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 0.400 GPa | 58.0 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, Conditioned Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This.. |