Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 200 cc/m²/day | 12.9 cc/100 in²/day | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |