Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name A-Series
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries.
Physical Properties Metric English Comments
Bulk Density 0.800 g/cc
0.0289 lb/in³
Bulk Density measured via tamp density method after 1500 tamps
1.80 g/cc
0.0650 lb/in³
Effective Density measured in SAE 20 motor oil using Gardner cup
Density 2.10 g/cc
0.0759 lb/in³
True Density measured via nitrogen gas displacement pycnometer
Brightness >= 95 %
>= 95 %
Hunter Whiteness
Oil Absorption 0.22 %
0.22 %
By mass (g oil/g spheres)
Particle Size >= 3.0 µm
>= 3.0 µm
D10
5.0 µm
5.0 µm
Mean, measured using laser light scattering
5.0 µm
5.0 µm
D50
<= 20 µm
<= 20 µm
D90
<= 25 µm
<= 25 µm
D97
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0
6.0
Compressive Strength >= 414 MPa
>= 60000 psi
Descriptive Properties Value Comments
Color White
Shape spherical