Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.0 MPa

@Temperature 23.0 °C
5220 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break >= 50 %

@Temperature 23.0 °C
>= 50 %

@Temperature 73.4 °F
DAM; nominal; ISO 527
170 %

@Temperature 23.0 °C
170 %

@Temperature 73.4 °F
DAM; nominal; ISO 527
200 %

@Temperature 23.0 °C
200 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 0.930 GPa

@Temperature 23.0 °C
135 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Modulus 0.980 GPa

@Temperature 23.0 °C
142 ksi

@Temperature 73.4 °F
DAM; ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
DAM; ISO 180/1A
95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact, Notched 3.00 J/cm²

@Temperature -40.0 °C
14.3 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 285 °C
545 °F
DAM; Optimum; Injection Molding
275 - 295 °C
527 - 563 °F
DAM; Injection Molding
Mold Temperature 60.0 °C
140 °F
DAM; optimum; Injection Molding
40.0 - 80.0 °C
104 - 176 °F
DAM; Injection Molding
Drying Temperature 80.0 °C
176 °F
DAM; Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM; Injection Molding
Moisture Content <= 0.20 %
<= 0.20 %
DAM; Injection Molding
Descriptive Properties Value Comments
Appearance Black Color
DAM
Forms Pellets
DAM
Generic Nylon 66
DAM
Material Status Current
DAM
Part Marking Code >PA66-F<
ISO 11469; DAM
Processing Method Injection Molding
DAM
Product Category Extrusion Resins
DAM
Toughened Resins
DAM
Unreinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA66-F
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM