Polymer Property : Tensile Modulus = 135 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.931 GPa
135 ksi
50mm/min; ASTM D638
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Tensile Modulus 0.931 - 1.14 GPa
135 - 165 ksi
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
Tensile Modulus 0.930 GPa
135 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus >= 0.930 GPa
>= 135 ksi
1 mm/min; ISO 527
MTM Plastics Dipolen® SP Recycled PP Blend
Dipolen® SP is a granulated polypropylene with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to custo..
Tensile Modulus 0.930 GPa
135 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP)
LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers.
Tensile Modulus 0.930 GPa

@Temperature 23.0 °C
135 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Tensile Modulus 0.930 GPa
135 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010  (Unverified Data**)
Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i..