Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.980 GPa | 142 ksi | Compression Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Flexural Modulus | 0.980 GPa @Temperature 90.0 °C |
142 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | Compression Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific) LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | ASTM D790 |
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.980 GPa @Temperature 23.0 °C |
142 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66
(Unverified Data**) Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | ASTM D790 |
Ashley Polymers Ashlene® 935-40M Nylon 11 A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer |
|||
Flexural Modulus | 0.980 GPa | 142 ksi | ISO 178 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |