Polymer Property : Charpy Impact, Notched = 10.5 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eA
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Charpy Impact, Notched 10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers