Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 70GB30HSL NC010 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® 70GB30HSL NC010 is a 30% glass bead reinforced heat stabilized polyamide 66 resin.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 2.00 mm
0.011 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
DAM; ISO 527
Flexural Modulus 4.20 GPa

@Temperature 23.0 °C
609 ksi

@Temperature 73.4 °F
DAM; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched 2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
10°C/min; DAM; ISO 11357-1/-3
Glass Transition Temp, Tg 80.0 °C
176 °F
10°C/min; DAM; ISO 11357-1/-2
Processing Properties Metric English Comments
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Forms Pellets
DAM
Generic PA66
DAM
Material Status Preliminary Data
DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Low Warp Resins
DAM
RoHS Compliance Contact Manufacturer
DAM
Users viewing this material also viewed the following: