Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.36 g/cc | 0.0491 lb/in³ | STN EN ISO 1183-1 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | DIN 53479 |
Qualchem Danamid FGFHUV-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial light.Information provided by Qualchem Zrt. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.36 g/cc | 0.0492 lb/in³ | |
Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul.. |
|||
Density | 1.36 g/cc | 0.0492 lb/in³ | |
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Plenco 2567 Phenolic, Granular, Injection Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Washington Penn Homopolymer Polypropylene 50% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792, ISO 1183 |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/A |
Addiplast Addinyl A2 M20 V10 Nylon 66, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/A |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1138 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU) Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |