Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos Styrenics Polystyrene 145D (NAFTA)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Ineos Styrenics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Styrenics Polystyrene 145D (NAFTA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 74
74
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 2.38 GPa
345 ksi
Flexural Modulus 3.03 GPa
439 ksi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
Vicat Softening Point 96.0 °C
205 °F
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Extrusion
180 - 280 °C
356 - 536 °F
Molding