Material Notes:
% Glass Reinforced, % Mineral Reinforced, Heat Stabilized
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
dry; ISO 1183
Moisture Absorption 1.50 %
1.50 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
cond; ISO 527-1/-2
95.0 MPa
13800 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
3.6 %
3.6 %
cond; ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
cond; ISO 527-1/-2
8.00 GPa
1160 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eU
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
0.530 J/cm²

@Temperature 23.0 °C
2.52 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 250 °C
482 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
dry; ISO 75-1/-2