Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.530 J/cm² @Temperature 23.0 °C |
2.52 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 0.530 J/cm² @Temperature 23.0 °C |
2.52 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 0.530 J/cm² @Temperature -30.0 °C |
2.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Charpy Impact, Notched | 0.530 J/cm² @Temperature -30.0 °C |
2.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Charpy Impact, Notched | 0.530 J/cm² @Temperature -30.0 °C |
2.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Charpy Impact, Notched | 0.530 J/cm² @Temperature -30.0 °C |
2.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |