Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 15 Polyamide 66, 15% Glass Fiber FeaturesChemically reinforced with 15% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S RCV3015 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 20 Polypropylene Homopolymer, 20% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 179-1eU |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber PBT, 7% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free) |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Stanyl® 46SF5030 PA46-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® B434 SE PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |