Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Borealis
Trade Name BorSafe™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. BorSafe™ ME3420 is classified as an MRS 8.0 material (PE80). Applications: BorSafe™ ME3420 is recommended for pressure pipe systems in the applications field of: drinking water, natural gas, industrial, relining, geothermal collector, and irrigation particularly where flexibility and coil ability is of importance. Thanks to its bimodal structure, it also shows excellent resistance to rapid crack propagation and slow crack growth.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 5.0 hour

@Pressure 0.800 MPa,
Temperature 80.0 °C
>= 5.0 hour

@Pressure 116 psi,
Temperature 176 °F
ISO 13479
Oxidative Induction Time (OIT) >= 20 min

@Temperature 200 °C
>= 20 min

@Temperature 392 °F
EN 728
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
50mm/min; ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Processing Properties Metric English Comments
Middle Barrel Temperature 180 - 210 °C
356 - 410 °F
cylinder
Die Temperature 200 - 210 °C
392 - 410 °F
Melt Temperature 200 - 220 °C
392 - 428 °F
Head Temperature 200 - 210 °C
392 - 410 °F
Descriptive Properties Value Comments
Resistance To Rapid Crack Propagation (bar) 7
S4 test, Pc at 0°C, test pipe 250mm, SDR11, ISO 13477