Physical Properties Metric English Comments
Environmental Stress Crack Resistance <= 5.0 hour
<= 5.0 hour
F50, Condition A; ASTM D-1693
ExxonMobil Escorene® LD-402 LDPE Electrical Jacketing Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low density polyethylene homopolymer resin designed for high speed extrusions.
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
Condition B, 10%, F50; ASTM D1693
Ineos T50-800 HDPE
T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use ..
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
Condition B, 10%, F50; ASTM D1693
Ineos T50-800-01 Polyethylene Copolymer
This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro..
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
Condition B, 10%, F50; ASTM D1693
Ineos T60-500 HDPE
T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog..
Environmental Stress Crack Resistance 5.0 hour

@Pressure 3.50 MPa
5.0 hour

@Pressure 508 psi
ISO CD 16770
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer..
Environmental Stress Crack Resistance 5.0 hour

@Pressure 3.50 MPa
5.0 hour

@Pressure 508 psi
ISO CD 16770
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene
BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo..
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
F<sub>50</sub>; ASTM D1693
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene
HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap..
Environmental Stress Crack Resistance >= 5.0 hour

@Pressure 0.920 MPa,
Temperature 80.0 °C
>= 5.0 hour

@Pressure 133 psi,
Temperature 176 °F
ISO 13479
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes
BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s..
Environmental Stress Crack Resistance >= 5.0 hour

@Pressure 0.800 MPa,
Temperature 80.0 °C
>= 5.0 hour

@Pressure 116 psi,
Temperature 176 °F
ISO 13479
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes
BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an ..
Environmental Stress Crack Resistance >= 5.0 hour

@Temperature 50.0 °C
>= 5.0 hour

@Temperature 122 °F
Igepal 10%;F0; IEC 60811-4-1/B
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables
Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®..
Environmental Stress Crack Resistance >= 5.0 hour

@Temperature 50.0 °C
>= 5.0 hour

@Temperature 122 °F
Igepal 10%, F0; IEC 60811-4-1/B
Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borstar® LE8706 is a natural colorable linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar technology allows ..
Environmental Stress Crack Resistance >= 5.0 hour

@Pressure 0.920 MPa,
Temperature 80.0 °C
>= 5.0 hour

@Pressure 133 psi,
Temperature 176 °F
ISO 13479
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s..
Environmental Stress Crack Resistance >= 5.0 hour
>= 5.0 hour
F50; ASTM D1693
CPC - Vycom POLYCARVE™ Coextruded High Density Sheet (HDPE)
PolyCarve™ thermoplastic engraving sign stock made to permanently resist the destructive outdoor elements, and certain indoor environments. PolyCarve is a high density, UV stabilized polyethylene c..
Environmental Stress Crack Resistance >= 5.0 hour

@Temperature 50.0 °C
>= 5.0 hour

@Temperature 122 °F
Igepal 10%, F0; IEC 60811-4-1/B
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa..