| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Bhansali Engineering Santron IMS1000 Sparkle SAN Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
| Melt Flow | 35.0 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
35.0 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Yield | 63.7 MPa <br>@Thickness 3.20 mm |
9250 psi <br>@Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
| 68.6 MPa <br>@Thickness 3.20 mm |
9960 psi <br>@Thickness 0.126 in |
Type I, 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 98.1 MPa <br>@Thickness 6.40 mm |
14200 psi <br>@Thickness 0.252 in |
5 mm/min; ASTM D790 |
| Izod Impact, Notched | 0.294 J/cm <br>@Thickness 3.20 mm |
0.551 ft-lb/in <br>@Thickness 0.126 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C <br>@Thickness 6.40 mm |
203 °F <br>@Thickness 0.252 in |
Method A; ASTM D648 |
| Flammability, UL94 | HB <br>@Thickness 3.20 mm |
HB <br>@Thickness 0.126 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90.0 % | 90.0 % | transparent; thickness not quantified |