Reliance Industries Polypropylene - 40% Glass filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Polypropylene - 40% Glass filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Reliance Industries
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
Tensile Modulus 5.52 GPa
801 ksi
Flexural Strength 165 MPa
23900 psi
Flexural Modulus 5.52 GPa
801 ksi
Izod Impact, Notched 7.52 J/cm
14.1 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F