Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Owens Corning Glass Fiber Reinforced Polyester (PET), 30 wt.% glass

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Owens Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polyester (PET), 30 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyesters are resistant to most organic solvents, weak acids and alkalis. They are not recommended with strong acids and alkalis or for prolonged use in hot water. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 140 MPa
20300 psi
ASTM D638
Elongation at Break 6.6 %
6.6 %
ASTM D638
Modulus of Elasticity 9.00 GPa
1310 ksi
ASTM D638
Flexural Strength 220 MPa
31900 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Compressive Strength 170 MPa
24700 psi
ASTM D695
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.6

@Frequency 60 Hz
3.6

@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.5 kV/mm
520 kV/in
ASTM D149
Arc Resistance 90 sec
90 sec
ASTM D495