Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |