Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene Moplen HP563S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP563S is a homopolymer typically used in spunb.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP601N Injection Molding Grade Polypropylene Moplen HP601N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP601N is a homopolymer typically used by customers in Glass Mat Sh.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP602N Injection Molding Grade Polypropylene Moplen HP602N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP602N is a homopolymer particularly suitable for injection molding.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP652P Fiber (BCF/CF) Grade Polypropylene Moplen HP652P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP652P is a homopolymer particularly suitable for heavy denier BCF .. |
|||
Izod Impact, Notched | >= 0.294 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.551 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3300 PP+MF30% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG3250A PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 23.0 °C |
0.551 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H1500 Polypropylene Homopolymer Features: SEETEC H1500 is a high flow homopolymer suitable for injection molding applications. SEETEC H1500 exhibits a high flowability combined with a good mechanical property balance. SEETEC H1500.. |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 23.0 °C |
0.551 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Izod Impact, Notched | >= 0.294 J/cm @Thickness 6.35 mm |
>= 0.551 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Engine Cover and Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | |
Shinil Chemical SHINSTAT MS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | |
Shinil Chemical SHINSTAT PP Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm |
0.551 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | >= 0.294 J/cm @Temperature 23.0 °C |
>= 0.551 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.550 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.550 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |