Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 35.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
35.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1465 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Uses: Sheet Forms: Pellets Processing Method: Injection Molding; Sheet .. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2448G Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2570A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2570F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2575A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2575F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 35.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
35.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
RTP Company RTP 199 X 137777 C Polypropylene (PP) Co-Polymer - High Flow - High Impact - Flame Retardant - UV Stabilized |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Melt Flow | 35.0 g/10 min @Load 10.0 kg, Temperature 250 °C |
35.0 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D 1238 |
RTP Company RTP 2099 X 134514 Polycarbonate/Polyester Flame Retardant - UV Stabilized - Chemical Resistant Alloy |