Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.04 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.35 mm |
4.04 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.35 mm |
4.04 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.35 mm |
4.04 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.35 mm |
4.04 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.16 J/cm @Thickness 6.40 mm |
4.04 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |