Polymer Property : Flexural Modulus = 320 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural
Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black
Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products HP514-447 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9902 Very Dark Gray
Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers PC-2109
Description: Natural Flame Retardant PolycarbonateInformation provided by Network Polymers Inc.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant
Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources ABS-FR1 ABS, Flame Retardant
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D 790
RTP Company RTP 300 TFE 15 Polycarbonate (PC), PTFE Lubricated
Flexural Modulus 2.21 GPa
320 ksi
ASTM D 790
RTP Company RTP 800 TFE 15 Acetal (POM), PTFE Lubricated
Flexural Modulus 2.21 GPa
320 ksi
ASTM D 790
RTP Company RTP 800 TFE 15 Z Acetal (POM), PTFE Lubricated - FDA Compliant Ingredients
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 2.21 - 7.86 GPa
320 - 1140 ksi
Average value: 5.37 GPa Grade Count:15
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Entec.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Hyosung Topilene HJ700 PP
HJ700 High Isostatic PP HomopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceInformation provided by Hyosung Corporation
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Spartech Royalite DKE 400 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman 310 Utility Black PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D 790
RTP Company EMI 660.5 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Flexural Modulus 2.21 GPa

@Thickness 6.40 mm
320 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Flexural Modulus 2.21 GPa

@Thickness 6.40 mm
320 ksi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Modulus 2.21 GPa

@Thickness 6.40 mm
320 ksi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Flexural Modulus 2.21 GPa
320 ksi
ASTM D 790
RTP Company RTP 300 TFE 20 Polycarbonate (PC), PTFE Lubricated