Material Notes:
MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of its cast granular structure and stress relieving properties, MIC-6 allows high-speed metal removal with little, if any, of the distortion commonly inherent in long grained wrought, flat-rolled metals.Using proper aluminum machining methods, tolerances in the thousandths can be consistently maintained. MIC-6 is finished to 20 microinches typical on both sides. Thickness tolerances is within +/-.005" from nominal on 1/4"- 4".Flatness tolerance is maintained within .015" on 1/4"-5/8" thickness and .005" on 3/4"- 4" thickness. Thermal Cycling can be performed up to 800° F under controlled conditions.MIC-6 is produced by continuous casting with each thickness individually cast. By utilizing the most recent developments in casting techniques, the molten metal is continuously fed, eliminating defects from lapses and seams. Thermal gradients are stabilized since heat is removed from both plate surfaces at a balanced rate. The employment of a SNIF filtering and degassing system ensures an end product free of voids and impurities.Information provided by Alcoa.
Mechanical Properties Metric English Comments
Hardness, Brinell 65
65
Tensile Strength, Ultimate 165 MPa
23900 psi
Tensile Strength, Yield 105 MPa
15200 psi
Elongation at Break 3.0 %
3.0 %
Modulus of Elasticity 71.0 GPa
10300 ksi
Thermal Properties Metric English Comments
CTE, linear 23.6 µm/m-°C

@Temperature 20.0 - 100 °C
13.1 µin/in-°F

@Temperature 68.0 - 212 °F
24.5 µm/m-°C

@Temperature 20.0 - 200 °C
13.6 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 142 W/m-K
985 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 0.00000479 ohm-cm
0.00000479 ohm-cm