Polymer Property : Izod Impact, Notched = 2.16 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.04 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical XR404 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf..
Izod Impact, Notched 2.16 J/cm

@Thickness 6.35 mm
4.04 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade
Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.16 J/cm

@Thickness 6.35 mm
4.04 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.16 J/cm

@Thickness 6.35 mm
4.04 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade
Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.16 J/cm

@Thickness 6.35 mm
4.04 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.05 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.05 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® 300H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.05 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® 400H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron HR60N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade
High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron HR60N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade
High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade
Electroplating, High FlowInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.05 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Izod Impact, Notched 2.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.05 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® 500H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade
Electroplating, High FlowInformation provided by Bhansali
Izod Impact, Notched 2.16 J/cm

@Thickness 6.40 mm
4.04 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali