Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Bedford Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many chemicalsLight Weight- Weighs nearly 80% less than a steel profile of similar dimensionElectrically Non-ConductiveNon-MetallicLower Life Cycle CostNon-Leaching. Environmentally FriendlyDimensional StabilityInformation provided by Bedford Plastics.
Physical Properties Metric English Comments
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Water Absorption <= 0.45 %
<= 0.45 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Tensile Strength, Ultimate 48.3 MPa
7000 psi
Crosswise; ASTM D638
207 MPa
30000 psi
Lengthwise; ASTM D638
Tensile Modulus 5.52 GPa
800 ksi
Crosswise; ASTM D638
17.2 GPa
2500 ksi
Lengthwise; ASTM D638
Flexural Strength 68.9 MPa
10000 psi
Crosswise; ASTM D790
207 MPa
30000 psi
Lengthwise; ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
Crosswise; ASTM D790
12.4 GPa
1800 ksi
Lengthwise; ASTM D790
Compressive Strength 103 MPa
15000 psi
Crosswise; ASTM D635
207 MPa
30000 psi
Lengthwise; ASTM D635
Compressive Modulus 6.89 GPa
1000 ksi
Crosswise; ASTM D635
17.2 GPa
2500 ksi
Lengthwise; ASTM D635
Shear Modulus 3.10 GPa
450 ksi
Shear Strength 31.0 MPa
4500 psi
Short Beam Shear; ASTM D2344
68.9 MPa
10000 psi
Punch Shear; ASTM D732
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
Crosswise; ASTM D256
13.3 J/cm
25.0 ft-lb/in
Lengthwise; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C

@Temperature 20.0 °C
4.44 µin/in-°F

@Temperature 68.0 °F
Lengthwise; ASTM D696
Electrical Properties Metric English Comments
Dielectric Constant 5.0

@Frequency 60 Hz
5.0

@Frequency 60 Hz
Perpendicular to Laminate Face; ASTM D150
Dielectric Strength 1.38 kV/mm
35.0 kV/in
Lengthwise; ASTM D149
7.87 kV/mm
200 kV/in
Perpendicular to Laminate Face; ASTM D149
Arc Resistance 120 sec
120 sec
Lengthwise; ASTM D495
Copyright © lookpolymers.com All Rights Reserved