Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.52 GPa | 800 ksi | ASTM D638 |
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet) |
|||
Tensile Modulus | 5.52 GPa | 800 ksi | |
MTI ThermoStran® PP-30G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |