Mechanical Properties Metric English Comments
Shear Modulus 3.10 GPa
450 ksi
in plane
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP
SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir..
Shear Modulus 3.10 GPa
450 ksi
in plane
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP
SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for ..
Shear Modulus 3.10 GPa
450 ksi
in plane
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP
SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted ..
Shear Modulus 3.10 GPa
450 ksi
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Shear Modulus 3.10 GPa
450 ksi
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Shear Modulus 3.10 GPa
450 ksi
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Shear Modulus 3.10 - 5.19 GPa
450 - 753 ksi
Average value: 4.40 GPa Grade Count:3
Overview of materials for Vinyl Ester Sheet Molding Compound