Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
PolyOne Edgetek® AS-10CF/000 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 GF25 FR IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame Retardant and Impact ModifierFeatures: Flame Retardant and Impact Modifi.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 HS L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PBT GF20 BK007 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 6225111Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PES GM20 WT139 20% Milled Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |