Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Multibase Nylex™ 4032 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D412 |
1085A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 48.3 - 103 MPa | 7000 - 15000 psi | Average value: 79.0 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Ultimate | 48.3 - 145 MPa | 7000 - 21000 psi | Average value: 84.8 MPa Grade Count:33 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 48.3 - 138 MPa | 7000 - 20000 psi | Average value: 88.2 MPa Grade Count:45 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 48 MPa | 7000 psi | ASTM D638 |
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 1080 DVD Polycarbonate CALIBREâ„¢ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D412 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | at 0.2"/min; ASTM D638 |
CPC - Vycom FLAMETEC™ CLEANROOM PVC-C Sheet Material Cleanroom PVC-C sheet material is designed to be the most economical choice in FM 4910 materials. Compression Polymers Corp's Cleanroom PVC-C has been audited and tested in accordance with the FM 49.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | |
Cotronics 4420 One-Part Epoxy |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Colorite Polymers 2010 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Applied Composites 8033 Polyester SMC Industry Application: RecreationProduct Application: Sports EquipmentDistinct Features: Pigmentable, Low Cost, Good Weatherability, High Molding EfficiencyInformation provided by Applied Composites .. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Applied Composites 8092 Polyester SMC Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo.. |
|||
Tensile Strength, Ultimate | 48.3 - 58.6 MPa | 7000 - 8500 psi | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Tensile Strength, Ultimate | 48.3 - 68.9 MPa | 7000 - 10000 psi | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | TM R050-36 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |