Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 150 Wicking Adhesive High Pressure Sealant Seals pores in welds and hairline cracks in castings |
|||
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 420 Instant High Pressure Pipe Sealant Industrial grade, controlled locking strength for metal fittings |
|||
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 440 High pressure Sealant Pneumatic and hydraulic sealant fluid, for power and gas system connections |
|||
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 444 High pressure Sealant Very high strength hydraulic sealant. Non-shrink, high vibration and shock resistance |
|||
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 446 High pressure Sealant Very high strength refrigerant sealant. Maximum solvent resistance |
|||
Shear Strength | >= 68.9 MPa | >= 10000 psi | |
ND Industries 460 Instant High Pressure Pipe Sealant High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings |
|||
Shear Strength | 68.9 MPa @Temperature 22.8 °C |
10000 psi @Temperature 73.0 °F |
ASTM D790 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Shear Strength | 68.9 - 186 MPa | 10000 - 27000 psi | Average value: 99.4 MPa Grade Count:9 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Shear Strength | 69.0 MPa | 10000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH
(disc AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Shear Strength | 68.9 MPa | 10000 psi | |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Shear Strength | 68.9 - 75.8 MPa | 10000 - 11000 psi | ASTM D732 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Shear Strength | 68.9 - 82.7 MPa | 10000 - 12000 psi | ASTM D732 |
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | Transverse; ASTM D732 |
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | ASTM D732 |
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced |
|||
Shear Strength | 69.0 MPa | 10000 psi | |
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | Punch Shear; ASTM D732 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | Punch Shear; ASTM D732 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 68.9 MPa | 10000 psi | Punch Shear; ASTM D732 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 69.2 MPa | 10000 psi | ILSS; EN2563 |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel |
|||
Shear Strength | 68.9 MPa | 10000 psi | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Shear Strength | 69.0 MPa | 10000 psi | ASTM D732 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |