Mechanical Properties Metric English Comments
Shear Strength 31.0 MPa
4500 psi
Die
Parker Chomerics CHO-BOND SV713 Conductive Epoxy
CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. ..
Shear Strength 31.0 MPa
4500 psi
Resinlab® RC8038 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Shear Strength 31.0 MPa
4500 psi
Interlaminar shear.
Type P-VSB-32 (Union Carbide) Carbon Fiber
Pitch fibers are prepared by heating aromatic compounds above 350°C. A dehydrogenation condensation reaction occurs to form planar aromatic molecules which aggregate into a liquid crystalline phas..
Shear Strength 31.0 MPa
4500 psi
ASTM D732
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
Shear Strength 31.0 MPa

@Temperature 21.1 °C
4500 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 609U Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Shear Strength 31.0 MPa

@Temperature 150 °C
4500 psi

@Temperature 302 °F
90º, ILSS Short Beam, Wet; EN2563
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Information provided by HexCel
Shear Strength 31.0 MPa
4500 psi
Short Beam Shear; ASTM D2344
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Shear Strength 31.0 MPa
4500 psi
Short Beam Shear; ASTM D2344
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Shear Strength 31.0 MPa
4500 psi
Short Beam Shear; ASTM D2344
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Shear Strength 31.0 MPa
4500 psi
Overlap, Aluminum Etched
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
Aluminum Overlap
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa

@Temperature -55.0 °C
4500 psi

@Temperature -67.0 °F
Aluminum Overlap
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa
4500 psi
Overlap, Aluminum Etched
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 31.0 MPa
4500 psi
Overlap, Aluminum Etched
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
Aluminum, Overlap
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 31.0 MPa

@Temperature -55.0 °C
4500 psi

@Temperature -67.0 °F
Aluminum, Overlap
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 31.0 MPa
4500 psi
Overlap, Etched Aluminum, RT, DI Water 30 days immersion, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 31.0 MPa
4500 psi
Overlap, Etched Aluminum, 10W30 Motor Oil at RT for 30 days immersion, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 31.0 MPa
4500 psi
Overlap, Etched Aluminum, -40°C/38°C and 100% RH/90°C; for 30 days, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 31.0 MPa
4500 psi
Aluminum, etched, Overlap, 30 day 65°C/80% RH, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
Aluminum, etched, Overlap, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
Aluminum, etched, Overlap, Cohesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..
Shear Strength 31.0 MPa
4500 psi
Overlap, Aluminum Etched
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa
4500 psi
Overlap, Isopropyl Alcohol immersion, RT for 30 days
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa

@Temperature -55.0 °C
4500 psi

@Temperature -67.0 °F
Aluminum Overlap
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
Aluminum Overlap
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 31.0 - 96.5 MPa
4500 - 14000 psi
Average value: 49.4 MPa Grade Count:5
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..