Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | Ultimate; TM R050-38 |
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Compressive Strength | 103 MPa | 15000 psi | Break; TM R050-38 |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Break; TM R050-38 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 103 - 124 MPa | 15000 - 18000 psi | ASTM D695 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE |
|||
Compressive Strength | >= 103 MPa | >= 15000 psi | |
Master Bond EP21SC-1 Two Component Epoxy Resin System Product Description: Master Bond Polymer System EP21SC-1 is a two component epoxy system featuring abrasion resistance. This high performance compound utilizes silicon carbide as a filler material a.. |
|||
Compressive Strength | >= 103 MPa | >= 15000 psi | |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Compressive Strength | 103 MPa | 15000 psi | |
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abra.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 103 - 117 MPa | 15000 - 17000 psi | |
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.Product Features:Combines good.. |
|||
Compressive Strength | 103 - 117 MPa | 15000 - 17000 psi | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Compressive Strength | 103 - 131 MPa | 15000 - 19000 psi | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Compressive Strength | 103 MPa | 15000 psi | Break; TM R050-38 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Compressive Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |