Arkema Group Rilsan® AESN P302 TL Nylon 12, Flexible Tubing Grade (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® AESN P302 TL Nylon 12, Flexible Tubing Grade (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
(Former designation: RILSAN MA 4403)Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and thermal stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance.Example applications: Tubes for air brake applications for trucks. approved by ISO 7628, DIN 73378 (PA12-HIPHL), NFR 12632, SAEJ 844.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 27 %
27 %
50 mm/min
Tensile Modulus 0.475 GPa
68.9 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 4.56 J/cm²
21.7 ft-lb/in²
Partial Break
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.14e+14 ohm-cm
1.14e+14 ohm-cm
Surface Resistance 7.74e+13 ohm
7.74e+13 ohm
Dielectric Strength 40.7 kV/mm
1030 kV/in
Comparative Tracking Index 600 V
600 V