Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PTS Trilac® TR558-CL ABS- Transparent ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name Trilac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS Trilac® TR558-CL ABS- Transparent ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 55.2 MPa
8010 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Yield Strength 90.3 MPa
13100 psi
ASTM D790
Flexural Modulus 2.65 GPa
384 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm

@Thickness 3.17 mm
1.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
Optical Properties Metric English Comments
Transmission, Visible 85 %
85 %
Transparent, but thickness unknown
Users viewing this material also viewed the following: