Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ISO 75 method A
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ISO 75-1/-2
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Compression Molded; ASTM D648
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Compression Molded; ASTM D648
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade
Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade
Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade
Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade
Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
LyondellBasell Lupolen® 5261 Z HI HDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ISO 75
Manifattura Cattaneo PE HD Polyethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific)
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP TH0815A
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C

@Thickness 3.20 mm
111 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp MK001AS PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MK001AS is a compound based on Polypropylene resin containing Mineral. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM D648
A. Schulman POLYFORT™ PP 3701
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM D648
A. Schulman POLYFORT™ PP 3701
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM D648
A. Schulman POLYFORT™ PP 3701
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Unannealed; 54°C (129°F) annealed; ASTM Data
Dow Prevail® 3050 ABS + Polyurethane
PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding
Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM-D648
Braskem Prisma 2910 RACO Random Polypropylene Copolymer
Prisma 2910 is a high melt flow rate random copolymer designed for injection molding applications. This product offers high impact strength at low temperatures and excellent processability. Its appl..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
Arkema Group Rilsan® AESN P302 TL Nylon 12, Flexible Tubing Grade (Dry)
(Former designation: RILSAN MA 4403)Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and thermal stabilized.Flexibility. High burst pressure a..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
BASF Novolen® 3300 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ISO 75
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good pro..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C
111 °F
ASTM D648
A. Schulman POLYFORT™ PP 3701
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 44.0 - 84.0 °C
111 - 183 °F
Average value: 64.6 °C Grade Count:3
Overview of materials for ABS/Polyurethane Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 - 150 °C
111 - 302 °F
Average value: 69.7 °C Grade Count:192